this post was submitted on 05 Sep 2025
24 points (96.2% liked)

3DPrinting

23494 readers
10 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 3 years ago
MODERATORS
 

I've mostly gotten the quality to where I'm happy except for whatever it's doing to the bow of Benchy. Still some stringing but I don't expect that to go away completely with TPU. Hatchbox TPU, been lowering temp, lowering print speed, fine tuning retraction, etc. I can give exact numbers if needed, but if anyone knows what to adjust specifically for what it's doing at the bow that would be great.

you are viewing a single comment's thread
view the rest of the comments
[–] morbidcactus@lemmy.ca 1 points 11 months ago

It'll cause more zits and the like, more stringing, don't know that'd 100% cause the issue but certainly won't help.

I just did a round of nylon last week which is also super hygroscopic, bag's like at most 8 months old but seal was intact. Even printing out of a drybox with fresh desiccant I noticed more stringing and occasional blobs + nozzle buildup over the few days (Was redoing my hotend so I inspected it, no sign of nozzle leaking), can definitely make overhangs worse.